On Jan 31, 2005, at 2:01 AM, chenysh wrote:
> Who can tell me the "sigma phase" in metal material at high temperture?
It's a chromium-rich area that forms in grain boundaries when
austenitic stainless cools too slowly through about 800 F. It promotes
intergranular corrosion.
Christopher Wright P.E. |"They couldn't hit an elephant at
chrisw@skypoint.com | this distance" (last words of Gen.
.......................................| John Sedgwick, Spotsylvania1864)