Re: Re: Reinforcement Pad Weep hole

From: <Christopher>
Date: Tue Sep 13 2005 - 12:04:00 EDT


On Sep 13, 2005, at 12:53 AM, tomcruz55 wrote:

> A RP was welded without the
> weep hole. Pad bulges.

Are you sure it bulges from trapped air or from welding heat distortion? The faying surface beween a pad and the vessel wall can't possibly trap air until the last bit of weld is applied, and if the air is warm, it soom cools. Takes a helluva lot of pressure to bulge a doubler plate.
Christopher Wright P.E. |"They couldn't hit an elephant at <a href="/group/PipingDesign/post?postID=D4Qdkcd2mNkvV_a1rcg0x5sv0jwnSDCaBCLYrL7xSL0z2K7dU5USupk69hPoqvPl_aBrFq0rxET3FAtg">chrisw@skypoint.com</a> | this distance" (last words of Gen.

.......................................| John Sedgwick, Spotsylvania
1864)
<a href="http://www.skypoint.com/~chrisw/">http://www.skypoint.com/~chrisw/</a> Received on Tue Sep 13 12:04:00 2005