Hardness measurements after PWHT

From: <jesvilla>
Date: Sat May 10 2008 - 16:18:00 EDT

We are in the process of welding process piping carbon steel P1, 7/8" through 1.5" thickness. PWHT has been done and the question is, do we need to measure hardness at all ? or take some aleatory readings? Is 225 BHN good hardness value reading for these piping? Received on Sat May 10 16:18:00 2008